Corrosion of Carbon Steel with and without Aluminized Coating in (O, S, H)-containing Gases at 500-800oC
| DC Field | Value | Language |
|---|---|---|
| dc.contributor.author | 이동복 | - |
| dc.contributor.author | Waheed Ali Abro | - |
| dc.contributor.author | 이근상 | - |
| dc.contributor.author | Muhammad Ali Abro | - |
| dc.date.accessioned | 2022-07-14T07:26:44Z | - |
| dc.date.available | 2022-07-14T07:26:44Z | - |
| dc.date.issued | 2017-04 | - |
| dc.identifier.issn | 1225-8024 | - |
| dc.identifier.issn | 2288-8403 | - |
| dc.identifier.uri | https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/152557 | - |
| dc.description.abstract | The carbon steel formed the thick, somewhat porous, loosely adherent iron oxide scale when oxidized at 500-800oC for 15 h in air. It formed the thicker, more porous, nonadherent scale consisting of FeS plus iron oxides in Ar/1%SO2-mixed gas. It formed the much thicker, more porous, nonadherent scale consisting of FeS plus iron oxides in Ar/0.1% H2S-mixed gas. However, the aluminized carbon steel formed the thin, protective Al2O3 surface scale even in Ar/1%SO2-, and Ar/0.1%H2S-mixed gas. Aluminizing drastically improved the corrosion resistance in (O, S, H)-containing gas. | - |
| dc.format.extent | 6 | - |
| dc.language | 영어 | - |
| dc.language.iso | ENG | - |
| dc.publisher | 한국표면공학회 | - |
| dc.title | Corrosion of Carbon Steel with and without Aluminized Coating in (O, S, H)-containing Gases at 500-800oC | - |
| dc.type | Article | - |
| dc.publisher.location | 대한민국 | - |
| dc.identifier.doi | 10.5695/JKISE.2017.50.2.85 | - |
| dc.identifier.bibliographicCitation | 한국표면공학회지, v.50, no.2, pp 85 - 90 | - |
| dc.citation.title | 한국표면공학회지 | - |
| dc.citation.volume | 50 | - |
| dc.citation.number | 2 | - |
| dc.citation.startPage | 85 | - |
| dc.citation.endPage | 90 | - |
| dc.identifier.kciid | ART002221429 | - |
| dc.description.isOpenAccess | N | - |
| dc.description.journalRegisteredClass | kci | - |
| dc.subject.keywordAuthor | Carbon steel | - |
| dc.subject.keywordAuthor | Aluminizing | - |
| dc.subject.keywordAuthor | Oxidation | - |
| dc.subject.keywordAuthor | SO2 corrosion | - |
| dc.subject.keywordAuthor | H2S corrosion | - |
| dc.identifier.url | http://koreascience.or.kr/article/JAKO201717447649646.page | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
222, Wangsimni-ro, Seongdong-gu, Seoul, 04763, Korea+82-2-2220-1366
COPYRIGHT © 2024 HANYANG UNIVERSITY.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.