Detailed Information

Cited 0 time in webofscience Cited 0 time in scopus
Metadata Downloads

Biocompatibility of 4-META/MMA-TBB resin used as a dental luting agent

Authors
Nakagawa, KaoriSaita, MakikoIkeda, TakayukiHirota, MakotoPark, WonheeLee, Masaichi Chang-IlOgawa, Takahiro
Issue Date
Jul-2015
Publisher
MOSBY-ELSEVIER
Citation
JOURNAL OF PROSTHETIC DENTISTRY, v.114, no.1, pp.114 - 121
Indexed
SCIE
SCOPUS
Journal Title
JOURNAL OF PROSTHETIC DENTISTRY
Volume
114
Number
1
Start Page
114
End Page
121
URI
https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/156895
DOI
10.1016/j.prosdent.2014.10.016
ISSN
0022-3913
Abstract
Statement of problem. The bonding and biological properties of currently used luting/cementing materials need to be improved. 4-Acryloyloxyethyl trimellitate anhydride/methyl methacrylate-tri-n-butylborane (4-META/MMA-TBB) resin is primarily used for splinting mobile teeth or treating fractured teeth. It undergoes moisture-resistant polymerization and bonds strongly to dentin and metals. Purpose. The purpose of this in vitro study was to compare the biological and biochemical properties META/MMA-TBB resin with those of conventional polymethyl methacrylate (PMMA)-MMA resin and other currently used luting materials in order to determine whether it may be a viable dental luting agent. Material and methods. The degree of polymerization of 4-META/MMA-TBB resin, PMMA-MMA autopolymerizing resin, 10-methacryloyloxydecyl dihydrogen phosphate-dimethacrylate (MDP-DMA) adhesive resin, and a glass ionomer cement was measured by Fourier-transformed infrared spectroscopy. Free radical production during setting was evaluated by electron spin resonance (ESR) spectroscopy. Rat dental pulp cells cultured on these materials were examined for cell viability, attachment, proliferation, and functional phenotype. Results. The degree of polymerization of 4-META/MMA-TBB resin was 82% thirty minutes after preparation, compared to 66% for PMMA-MMA autopolymerizing resin. ESR spectroscopy revealed free radical production from 4-META/MMA-TBB resin and glass ionomer cement was equivalent 24 hours after preparation, with no spike in radical generation observed. In contrast, free radical production from PMMA-MMA and MDP-DMA adhesive resins was rapid and sustained and 10 to 20 times greater than that from 4-META/MMA-TBB. The percentage of viable dental pulp cells 24 hours after seeding was considerably higher on MDP-DMA and 4-META/MMA-TBB resin than on glass ionomer cement. Cell number, proliferation, and alkaline phosphatase activity were highest on 4-META/MMA-TBB resin and lowest on the glass ionomer cement. Conclusions. 4-META/MMA-TBB resin is at least as biocompatible, and perhaps even more biocompatible, than other current luting materials, with fast, favorable, and nontoxic polymerization properties. Further in vivo and human studies of 4-META/MMA-TBB resin as a dental luting agent are warranted.
Files in This Item
There are no files associated with this item.
Appears in
Collections
서울 의과대학 > 서울 치과학교실 > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Park, Won hee photo

Park, Won hee
COLLEGE OF MEDICINE (DEPARTMENT OF DENTISTRY)
Read more

Altmetrics

Total Views & Downloads

BROWSE