Electrical characteristics of resistive switching memory with metal oxide nanoparticles on a graphene layer
| DC Field | Value | Language |
|---|---|---|
| dc.contributor.author | Lee, Dong Uk | - |
| dc.contributor.author | Kim, Dongwook | - |
| dc.contributor.author | Kim, Eun Kyu | - |
| dc.contributor.author | Cho, Won-Ju | - |
| dc.contributor.author | Kim, Young-Ho | - |
| dc.contributor.author | Im, Hyunsik | - |
| dc.date.accessioned | 2022-07-16T08:32:13Z | - |
| dc.date.available | 2022-07-16T08:32:13Z | - |
| dc.date.issued | 2013-09 | - |
| dc.identifier.issn | 0040-6090 | - |
| dc.identifier.uri | https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/162090 | - |
| dc.description.abstract | A resistive switching memory device with SnO2 nanoparticles embedded in a biphenyl-tertracarboxylic dianhydride-phenylene diamine polyimide layer on single layered graphene (SLG) was demonstrated, and its electrical properties were characterized. Current levels in the resistance switching memory device were controlled by applying pulse voltages of +/- 10 V for 100 ms. The current values of high and low resistance states (HRS and LRS) at 1 V were measured to be about 4.60 x 10(-4) A and 3.04 x 10(-3) A, respectively. The ratio of the HRS and LRS after applying a pulse bias of +/- 10 V appeared to be about 7.9 at 1 V, and this result was retained after 10(4) s. The resistance switching may originate from carrier charging and recombination effects into the SnO2 nanoparticles through modulation of the Fermi level of the SLG due to the applied bias. | - |
| dc.format.extent | 4 | - |
| dc.language | 영어 | - |
| dc.language.iso | ENG | - |
| dc.publisher | Elsevier Sequoia | - |
| dc.title | Electrical characteristics of resistive switching memory with metal oxide nanoparticles on a graphene layer | - |
| dc.type | Article | - |
| dc.publisher.location | 스위스 | - |
| dc.identifier.doi | 10.1016/j.tsf.2013.02.111 | - |
| dc.identifier.scopusid | 2-s2.0-84883205687 | - |
| dc.identifier.wosid | 000324049500024 | - |
| dc.identifier.bibliographicCitation | Thin Solid Films, v.543, pp 106 - 109 | - |
| dc.citation.title | Thin Solid Films | - |
| dc.citation.volume | 543 | - |
| dc.citation.startPage | 106 | - |
| dc.citation.endPage | 109 | - |
| dc.type.docType | Article; Proceedings Paper | - |
| dc.description.isOpenAccess | N | - |
| dc.description.journalRegisteredClass | sci | - |
| dc.description.journalRegisteredClass | scie | - |
| dc.description.journalRegisteredClass | scopus | - |
| dc.relation.journalResearchArea | Materials Science | - |
| dc.relation.journalResearchArea | Physics | - |
| dc.relation.journalWebOfScienceCategory | Materials Science, Multidisciplinary | - |
| dc.relation.journalWebOfScienceCategory | Materials Science, Coatings & Films | - |
| dc.relation.journalWebOfScienceCategory | Physics, Applied | - |
| dc.relation.journalWebOfScienceCategory | Physics, Condensed Matter | - |
| dc.subject.keywordPlus | RAMAN-SPECTROSCOPY | - |
| dc.subject.keywordPlus | TRANSISTORS | - |
| dc.subject.keywordPlus | POLYIMIDE | - |
| dc.subject.keywordPlus | GROWTH | - |
| dc.subject.keywordAuthor | SnO2 | - |
| dc.subject.keywordAuthor | Resistance switching | - |
| dc.subject.keywordAuthor | Nonvolatile memory | - |
| dc.subject.keywordAuthor | Polyimide | - |
| dc.subject.keywordAuthor | Graphene | - |
| dc.identifier.url | https://www.sciencedirect.com/science/article/pii/S0040609013003817?via%3Dihub | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
222, Wangsimni-ro, Seongdong-gu, Seoul, 04763, Korea+82-2-2220-1366
COPYRIGHT © 2024 HANYANG UNIVERSITY.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.