Control of H2O generated during the CO2 hardening process in a casting mold
| DC Field | Value | Language |
|---|---|---|
| dc.contributor.author | Kim, Eun-Hee | - |
| dc.contributor.author | Lee, Je-Hyun | - |
| dc.contributor.author | Jung, Yeon-Gil | - |
| dc.contributor.author | Jang, Jung-Chel | - |
| dc.contributor.author | Paik, Ungyu | - |
| dc.date.accessioned | 2022-07-16T10:10:07Z | - |
| dc.date.available | 2022-07-16T10:10:07Z | - |
| dc.date.issued | 2013-05 | - |
| dc.identifier.issn | 0272-8842 | - |
| dc.identifier.issn | 1873-3956 | - |
| dc.identifier.uri | https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/162878 | - |
| dc.description.abstract | An additive reagent was introduced into a water glass binder system for enhancing the mechanical properties and dimension stability of a casting mold, and for improving the surface quality of a cast product. Two different processes with three different additive reagents were employed to investigate the relation between fracture strength of the mold and water (H2O) existed in the mold. In processes I and II, the mold samples were coated with a water glass binder, and then dipped into different solutions with additive reagent after and before carbon dioxide (CO2) hardening, respectively. The fracture strength of the mold was enhanced by reducing H2O content in the mold, achieved by a hydrolysis reaction of additive reagents. In process I, the H2O movement was restricted in the mold by the solid phase, converted from the water glass during CO2 hardening. When employing process II, especially in the TEOS used as additive reagent, the fracture strength was significantly increased due to the effective reduction of H2O content in the mold and the homogeneous generation of glass phase by a sol gel reaction of the additives. | - |
| dc.format.extent | 6 | - |
| dc.language | 영어 | - |
| dc.language.iso | ENG | - |
| dc.publisher | Elsevier | - |
| dc.title | Control of H2O generated during the CO2 hardening process in a casting mold | - |
| dc.type | Article | - |
| dc.publisher.location | 영국 | - |
| dc.identifier.doi | 10.1016/j.ceramint.2012.10.249 | - |
| dc.identifier.scopusid | 2-s2.0-84874653962 | - |
| dc.identifier.wosid | 000318129100069 | - |
| dc.identifier.bibliographicCitation | Ceramics International, v.39, no.4, pp 3993 - 3998 | - |
| dc.citation.title | Ceramics International | - |
| dc.citation.volume | 39 | - |
| dc.citation.number | 4 | - |
| dc.citation.startPage | 3993 | - |
| dc.citation.endPage | 3998 | - |
| dc.type.docType | Article | - |
| dc.description.isOpenAccess | N | - |
| dc.description.journalRegisteredClass | sci | - |
| dc.description.journalRegisteredClass | scie | - |
| dc.description.journalRegisteredClass | scopus | - |
| dc.relation.journalResearchArea | Materials Science | - |
| dc.relation.journalWebOfScienceCategory | Materials Science, Ceramics | - |
| dc.subject.keywordPlus | STEEL | - |
| dc.subject.keywordAuthor | Water glass | - |
| dc.subject.keywordAuthor | Additive reagent | - |
| dc.subject.keywordAuthor | Hydrolysis reaction | - |
| dc.subject.keywordAuthor | Fracture strength | - |
| dc.identifier.url | https://www.sciencedirect.com/science/article/pii/S0272884212012126?via%3Dihub | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
222, Wangsimni-ro, Seongdong-gu, Seoul, 04763, Korea+82-2-2220-1366
COPYRIGHT © 2024 HANYANG UNIVERSITY.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.