Thermally Stable Biodegradable Polyesters with Camphor and Tartaric Acid Coupled Cyclic Diester Monomers for Controlled Hydrolytic Degradations

Authors
Kang, Ju HuiLee, Joon HyukLee, SangkugSuh, Dong HackYeom, Bongjun
Issue Date
Mar-2023
Publisher
AMER CHEMICAL SOC
Keywords
KEYWORDS; Polyester; biodegradation; tartaric acid; camphor; thermal stability; hydrolytic degradation
Citation
ACS APPLIED POLYMER MATERIALS, v.5, no.3, pp.1859 - 1870
Indexed
SCIE
SCOPUS
Journal Title
ACS APPLIED POLYMER MATERIALS
Volume
5
Number
3
Start Page
1859
End Page
1870
URI
https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/184947
DOI
10.1021/acsapm.2c01945
ISSN
2637-6105
Abstract
The development of biodegradable engineering plastics is challenging, because increases in biodegradability mostly degrade other material properties, such as mechanical and thermal properties of polymers. Here, we use bioderivatives of diester monomers, dimethyl (1S,4R)-1,7,7-trimethylspiro[bicyclo[2.2.1]heptane-2,2′-[1,3]dioxolane]-4′,5′-dicarboxylate (camphor dimethyl dl-tartrate, Ct diester), for the synthesis of phthalate-based copolyesters to enhance degradability without a notable loss of thermal stability. Ct diester synthesized by acetalization of tartaric acid and camphor contains a bridged type of rigid bicycling ring with high thermal stability and controlled degradation via hydrolysis of acetal groups within the spiro-ring structure. Various alkyl-length diols of ethylene, butylene, and hexylene are copolymerized with mixtures of dimethyl phthalate (DMT) and Ct diester in a 9:1 molar ratio. The glass transition temperature and degradation temperature of the copolyesters are comparable to those of DMT-based homopolyesters. Due to decreases in crystallinity, copolyesters exhibit slight decreases in melting temperature of 10 to 20 °C, which can be advantageous for reducing processing temperatures. Notably, the copolyesters demonstrate enhanced hydrolytic degradation of 9.3 to 26.2% in pH 2 environment for 18 days, as measured by the degree of molecular weight reductions. These values are between 1.7 and 3.5 times higher than the degradation rates of their control samples of DMT-based homopolyesters under the same degradation conditions.
Files in This Item
Go to Link
Appears in
Collections
서울 공과대학 > 서울 화학공학과 > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Yeom, Bong jun photo

Yeom, Bong jun
COLLEGE OF ENGINEERING (DEPARTMENT OF CHEMICAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE