| dc.description.abstract | Mo nanopowder was synthesized by ball-milling and subsequent hydrogen-reduction of MoO3 powder. After hydrogen-reduction at 800oC, the crystalline size of the Mo powder was about 60 nm. The sinterability of the Mo nanopowder was considerably enhanced compared with that of a commercial Mo power. The sintering behavior of Mo nanopowder was investigated in comparison to that of commercial Mo powder. At a sintering temperature of 1400oC, the relative density of Mo nanopowder (94%) was found to be higher than that of commercial powder (74%). | - |
| dc.title | synthesis of Mo nanopowder by mechanochemical process | - |
| dc.type | Conference | - |
| dc.citation.conferenceName | JSEM2007 | - |
| dc.citation.conferencePlace | busan youth hostel.(aspina) | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
222, Wangsimni-ro, Seongdong-gu, Seoul, 04763, Korea+82-2-2220-1366
COPYRIGHT © 2024 HANYANG UNIVERSITY.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.