Effects of Kenaf Fibers Coated with Aluminum Trihydroxide on Limiting Oxygen Index and Thermal and Mechanical Properties of Biocomposites
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Woo, Yeonhae | - |
dc.contributor.author | Cho, Donghwan | - |
dc.date.accessioned | 2024-02-27T13:00:35Z | - |
dc.date.available | 2024-02-27T13:00:35Z | - |
dc.date.issued | 2016-07 | - |
dc.identifier.issn | 0379-153X | - |
dc.identifier.issn | 2234-8077 | - |
dc.identifier.uri | https://scholarworks.bwise.kr/kumoh/handle/2020.sw.kumoh/26978 | - |
dc.description.abstract | The effects of aluminum trihydroxide (ATH) coating on kenaf fibers on the properties such as limiting oxygen index, thermal stability, thermal expansion, dynamic mechanical properties, and tensile properties of biocomposites composed of kenaf fibers and poly(lactic acid) (PLA) are studied. It has been found that with increasing the ATH coating concentration the kenaf fiber surfaces are changed and the surfaces become rougher as there is an increase in the surface area due to the distributed ATH particles. The ATH coating on the kenaf fibers results in the enhancement of not only limiting oxygen index (LOI), which is closely relevant to retardancy, but also thermal stability, thermo-dimensional stability, storage modulus, and tensile properties of kenaf fiber/PLA biocomposites, depending on the ATH coating concentration. ATH coating with an appropriate concentration significantly contributes to imparting fire resistance and also to reinforcing this biocomposite system. | - |
dc.format.extent | 9 | - |
dc.language | 한국어 | - |
dc.language.iso | KOR | - |
dc.publisher | POLYMER SOC KOREA | - |
dc.title | Effects of Kenaf Fibers Coated with Aluminum Trihydroxide on Limiting Oxygen Index and Thermal and Mechanical Properties of Biocomposites | - |
dc.type | Article | - |
dc.publisher.location | 대한민국 | - |
dc.identifier.doi | 10.7317/pk.2016.40.4.568 | - |
dc.identifier.wosid | 000380731900010 | - |
dc.identifier.bibliographicCitation | POLYMER-KOREA, v.40, no.4, pp 568 - 576 | - |
dc.citation.title | POLYMER-KOREA | - |
dc.citation.volume | 40 | - |
dc.citation.number | 4 | - |
dc.citation.startPage | 568 | - |
dc.citation.endPage | 576 | - |
dc.type.docType | Article | - |
dc.identifier.kciid | ART002128823 | - |
dc.description.isOpenAccess | N | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
dc.description.journalRegisteredClass | kci | - |
dc.relation.journalResearchArea | Polymer Science | - |
dc.relation.journalWebOfScienceCategory | Polymer Science | - |
dc.subject.keywordPlus | ELECTRON-BEAM IRRADIATION | - |
dc.subject.keywordPlus | SURFACE-TREATMENTS | - |
dc.subject.keywordPlus | SUCCINATE) BIOCOMPOSITES | - |
dc.subject.keywordPlus | BIODEGRADABLE POLYMERS | - |
dc.subject.keywordPlus | GREEN COMPOSITES | - |
dc.subject.keywordPlus | FLAME RETARDANTS | - |
dc.subject.keywordPlus | NATURAL FIBERS | - |
dc.subject.keywordPlus | JUTE | - |
dc.subject.keywordPlus | NANOCOMPOSITES | - |
dc.subject.keywordPlus | FLAMMABILITY | - |
dc.subject.keywordAuthor | biocomposites | - |
dc.subject.keywordAuthor | kenaf fiber | - |
dc.subject.keywordAuthor | poly(lactic acid) | - |
dc.subject.keywordAuthor | limiting oxygen index | - |
dc.subject.keywordAuthor | material properties | - |
dc.subject.keywordAuthor | aluminum trihydroxide coating | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
350-27, Gumi-daero, Gumi-si, Gyeongsangbuk-do, Republic of Korea (39253)054-478-7170
COPYRIGHT 2020 Kumoh University All Rights Reserved.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.