Tailoring interfacial stability with lithium salt additives for long-cycling Ni-rich cathodes in lithium metal batteries
DC Field | Value | Language |
---|---|---|
dc.contributor.author | 조국영 | - |
dc.date.accessioned | 2025-09-30T08:00:19Z | - |
dc.date.available | 2025-09-30T08:00:19Z | - |
dc.date.issued | 2025-10 | - |
dc.identifier.issn | 2468-0230 | - |
dc.identifier.issn | 2468-0230 | - |
dc.identifier.uri | https://scholarworks.bwise.kr/erica/handle/2021.sw.erica/126564 | - |
dc.description.abstract | The development of next-generation battery systems with high energy density is crucial for the advancement of electric vehicles (EVs). The combination of a high-nickel cathode with a lithium-metal anode is a particularly promising candidate for this application, as both materials demonstrate individually high theoretical specific capacities. However, each electrode presents intrinsic challenges that must be individually understood and synergistically mitigated to unlock their full potential. In this study, the effectiveness of various lithium salts as electrolyte additives for stabilizing LiNi0.8Co0.1Mn0.1O2 (NCM811) cathodes is investigated. A systematic comparison of lithium tetrafluoroborate, lithium bis(oxalate)borate, lithium difluoro(oxalate)borate (LiDFOB), lithium nonafluoro-1-butanesulfonate, lithium bis(trifluoromethanesulfonyl)imide, and lithium trimethylsilanolate (LiTMS) is conducted in a LiPF6-based electrolyte to evaluate their impact on interfacial chemistry and long-term cycling performance. Among the additives tested, LiDFOB demonstrates the most promising results, retaining approximately 70 % of its initial capacity after 400 cycles at 25 ◦C and 87.7 % at 50 ◦C. In contrast, while LiTMS initially appears effective in forming a protective cathode electrolyte interphase (CEI), it ultimately leads to significant impedance growth and capacity degradation over extended cycling. comprehensive electrochemical evaluations and ex situ characterizations reveal that the interfacial reactivity and integrity of the resulting CEI play a more critical role in determining long-term stability than the mechanical degradation traditionally attributed to particle cracking. These findings challenge the conventional emphasis on structural failure as the primary mode of degradation in high-Ni cathodes and underscore the significance of rational CEI design through electrolyte additive engineering | - |
dc.format.extent | 1 | - |
dc.language | 영어 | - |
dc.language.iso | ENG | - |
dc.publisher | ELSEVIER | - |
dc.title | Tailoring interfacial stability with lithium salt additives for long-cycling Ni-rich cathodes in lithium metal batteries | - |
dc.type | Article | - |
dc.publisher.location | 네델란드 | - |
dc.identifier.doi | 10.1016/j.surfin.2025.107707 | - |
dc.identifier.scopusid | 2-s2.0-105016791954 | - |
dc.identifier.bibliographicCitation | SURFACES AND INTERFACES, v.74, pp 107707 - 107707 | - |
dc.citation.title | SURFACES AND INTERFACES | - |
dc.citation.volume | 74 | - |
dc.citation.startPage | 107707 | - |
dc.citation.endPage | 107707 | - |
dc.type.docType | 정기학술지(Article(Perspective Article포함)) | - |
dc.description.isOpenAccess | N | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
dc.subject.keywordAuthor | Cathode Electrolyte Interphase | - |
dc.subject.keywordAuthor | Drt Analysis | - |
dc.subject.keywordAuthor | Electrolyte Additive | - |
dc.subject.keywordAuthor | High-nickel Cathode | - |
dc.subject.keywordAuthor | Particle Cracking | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
55 Hanyangdeahak-ro, Sangnok-gu, Ansan, Gyeonggi-do, 15588, Korea+82-31-400-4269 sweetbrain@hanyang.ac.kr
COPYRIGHT © 2021 HANYANG UNIVERSITY. ALL RIGHTS RESERVED.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.