Density Measurements of CaO-MnO-SiO2 Slags
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Lee, Joonho | - |
dc.contributor.author | Hoai, Le Thu | - |
dc.contributor.author | Choe, Joongkil | - |
dc.contributor.author | Park, Joo Hyun | - |
dc.date.accessioned | 2021-06-23T10:03:07Z | - |
dc.date.available | 2021-06-23T10:03:07Z | - |
dc.date.issued | 2012-00 | - |
dc.identifier.issn | 0915-1559 | - |
dc.identifier.issn | 1347-5460 | - |
dc.identifier.uri | https://scholarworks.bwise.kr/erica/handle/2021.sw.erica/36314 | - |
dc.description.abstract | Density measurements of CaO-MnO-SiO2 slags were carried out using the Archimedean method. The density decreased with increasing temperature, and the negative temperature coefficient (-d rho/dT) was in the range of 1.46-3.10 x 10(-1) kg/m(3) K. At a fixed CaO content (25 wt%) and at a fixed SiO2 content (30 wt%), the density of CaO-MnO-SiO2 slag increased with increasing MnO content. The molar volumes of CaO, MnO and SiO2 at 1 773 K were estimated 21.0, 17.2, and 28.0 x 10(-6) m(3)/mol, respectively. The molar excess volume was expressed by V-Ex = Omega AX(SiO2) (1-X-SiO2), where Omega = 8.97 x 10(-6) m(3)/mol at 1 773 K. The thermal expansion coefficient decreased with increasing m(3)/mol because of the enhanced silicate network structure. | - |
dc.format.extent | 4 | - |
dc.language | 영어 | - |
dc.language.iso | ENG | - |
dc.publisher | Nippon Tekko Kyokai/Iron and Steel Institute of Japan | - |
dc.title | Density Measurements of CaO-MnO-SiO2 Slags | - |
dc.type | Article | - |
dc.publisher.location | 일본 | - |
dc.identifier.doi | 10.2355/isijinternational.52.2145 | - |
dc.identifier.scopusid | 2-s2.0-84871733672 | - |
dc.identifier.wosid | 000312968000005 | - |
dc.identifier.bibliographicCitation | ISIJ International, v.52, no.12, pp 2145 - 2148 | - |
dc.citation.title | ISIJ International | - |
dc.citation.volume | 52 | - |
dc.citation.number | 12 | - |
dc.citation.startPage | 2145 | - |
dc.citation.endPage | 2148 | - |
dc.type.docType | Article | - |
dc.description.isOpenAccess | N | - |
dc.description.journalRegisteredClass | sci | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
dc.relation.journalResearchArea | Metallurgy & Metallurgical Engineering | - |
dc.relation.journalWebOfScienceCategory | Metallurgy & Metallurgical Engineering | - |
dc.subject.keywordPlus | CAO-SIO2-MNO SLAG | - |
dc.subject.keywordPlus | SURFACE-TENSION | - |
dc.subject.keywordPlus | MELTS | - |
dc.subject.keywordPlus | CAPACITY | - |
dc.subject.keywordPlus | MN | - |
dc.subject.keywordAuthor | Archimedean method | - |
dc.subject.keywordAuthor | CaO-MnO-SiO2 slag | - |
dc.subject.keywordAuthor | density | - |
dc.subject.keywordAuthor | molar volume | - |
dc.subject.keywordAuthor | silicate network structure | - |
dc.subject.keywordAuthor | thermal expansion coefficient | - |
dc.identifier.url | https://www.jstage.jst.go.jp/article/isijinternational/52/12/52_2145/_article | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
55 Hanyangdeahak-ro, Sangnok-gu, Ansan, Gyeonggi-do, 15588, Korea+82-31-400-4269 sweetbrain@hanyang.ac.kr
COPYRIGHT © 2021 HANYANG UNIVERSITY. ALL RIGHTS RESERVED.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.