Formation Mechanism of Spinel-type Inclusions in High Alloyed Stainless Steel Melts

Authors
박주현
Issue Date
Aug-2007
Publisher
ASM International
Keywords
Austenitic Stainless Steel; Continuous Casting; Calcium Silicate; Spinel Phase; Molten Steel
Citation
Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science, v.38, no.4, pp.657 - 663
Indexed
SCIE
Journal Title
Metallurgical and Materials Transactions B: Process Metallurgy and Materials Processing Science
Volume
38
Number
4
Start Page
657
End Page
663
URI
https://scholarworks.bwise.kr/erica/handle/2021.sw.erica/43518
DOI
10.1007/s11663-007-9066-x
ISSN
1073-5615
Abstract
Fundamental thermodynamics of the relationship between high-alloyed stainless steel melts (Fe-20 mass pet Cr-13 mass pct Ni-3 mass pct Si) and the inclusions were investigated. The formation mechanism of the inclusions containing the spinel crystals was developed based on the experimental results and from the compositions of the inclusions in the steel samples taken during plant operations. The molar content of alumina in the inclusions was found to be linearly proportional to the increase of aluminum content, indicating that the inclusions could contain alumina even with less than about 200 ppm aluminum in the steel melt, e.g., steel melts that were mainly deoxidized by silicon. Furthermore, the composition of the inclusions is shown to be a function of the activity of the deoxidizers such as aluminum and silicon in the steel melt. From the analysis of the plant samples, it was found that the contents of MgO and Al2O3 in the calcium silicate type inclusions increased continuously as the steel melt transfers from the argon oxygen decarburization (AOD) converter to the tundish. This composition change in the inclusions originated from the reduction of MgO and Al2O3 in the slags or refractories by silicon in the steel melt. Increases of MgO and Al2O3 contents were prominent in tundish samples, and thus, the spinel phase could be crystallized in the calcium silicate inclusion matrix in the tundish; and finally the spinel crystals grew during cooling of the steel melt through the continuous casting (CC) mold and in the slabs. On the other hand, manganese silicate type inclusions containing chromium oxide were observed after tapping of the molten steel to the ladle. The MnO and Cr2O3 in these inclusions was initially reduced by silicon in the steel melt in the ladle treatment (LT) process, followed by further reduction by aluminum through the LT to the CC mold. The fractions of inclusions containing spinel crystals in cast slabs were negligible at the alumina content of less than about 20 mass pct, while they critically increased at alumina contents greater than about 20 mass pct.
Files in This Item
Go to Link
Appears in
Collections
COLLEGE OF ENGINEERING SCIENCES > DEPARTMENT OF MATERIALS SCIENCE AND CHEMICAL ENGINEERING > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Park, Joo Hyun photo

Park, Joo Hyun
ERICA 공학대학 (DEPARTMENT OF MATERIALS SCIENCE AND CHEMICAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE