Effect of Sealing Time of Anodic Aluminum Oxide (AAO) Film for Preventing Plasma Damage

Authors
Song, Je-BoemKim, Jin-TaeOh, Seong-GeunShin, Jae-SooChun, Je-RanYun, Ju-Young
Issue Date
Jan-2015
Publisher
AMER SCIENTIFIC PUBLISHERS
Keywords
Aluminum Oxide; Sealing; Anodizing; Plasma Resistance; Contamination Particles
Citation
SCIENCE OF ADVANCED MATERIALS, v.7, no.1, pp.127 - 132
Indexed
SCIE
SCOPUS
Journal Title
SCIENCE OF ADVANCED MATERIALS
Volume
7
Number
1
Start Page
127
End Page
132
URI
https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/158152
DOI
10.1166/sam.2015.2091
ISSN
1947-2935
Abstract
The damage to the surface structure of Anodic Aluminum Oxide (AAO) caused by plasma and heat is evaluated with respect to the sealing time (0, 10, 30 and 60 minutes). With 10 minutes sealing time of the oxide layer, the leakage current is abruptly reduced, while the breakdown voltage and permittivity are rapidly improved. Longer sealing after 10 minutes makes less efficiencies. In the samples sealed for 30 or 60 minutes, more cracks are generated by plasma and heat treatments, result in the reduction of the breakdown voltage. Sealing longer than 10 minutes produces much contamination particles by plasma treatment. The resistance to plasma and heat is improved with a sealing time of 10 minutes.
Files in This Item
Go to Link
Appears in
Collections
서울 공과대학 > 서울 화학공학과 > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Oh, Seong-Geun photo

Oh, Seong-Geun
COLLEGE OF ENGINEERING (DEPARTMENT OF CHEMICAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE