Exploring the use of butadiene rubbers as a binder in composite cathodes for all-solid-state lithium batteries

Authors
Lee, Young-JunHong, Seung-BoKim, Dong Won
Issue Date
Jun-2023
Publisher
ELSEVIER SCIENCE INC
Keywords
All-solid-state lithium battery; Sulfide solid electrolyte; Polymer binder; Composite cathode; Wet-slurry process
Citation
JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY, v.122, no.25, pp.341 - 348
Indexed
SCIE
SCOPUS
KCI
Journal Title
JOURNAL OF INDUSTRIAL AND ENGINEERING CHEMISTRY
Volume
122
Number
25
Start Page
341
End Page
348
URI
https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/191594
DOI
10.1016/j.jiec.2023.02.034
ISSN
1226-086X
Abstract
Among the various next-generation battery systems, all-solid-state lithium batteries (ASSLBs) employing sulfide-based solid electrolytes have garnered considerable attention because of their high energy density and enhanced safety compared to conventional lithium-ion batteries (LIBs) with liquid electrolytes. The fabrication of composite cathodes for ASSLBs by the wet-slurry process is highly desirable, because it can be scaled into a large sheet and be applied to the established slurry-processed electrode manufacturing technology of LIBs. A polymer binder in the composite cathode is an important component for maintaining good interfacial contacts among the electrode components (active material, solid electrolyte, and conducting carbon) during charge and discharge cycles. In this study, we used polybutadiene and acrylonitrile-butadiene rubbers (NBR) with different acrylonitrile (AN) contents as a polymer binder in the composite cathode. Our results demonstrated that a composite cathode employing NBR with 25 wt.% AN (NBR25) showed good elastic properties and superior adhesion without the large deterioration of interfacial contacts during cycling. The solid-state Li-In/Li6PS5Cl/LiNi0.7Co0.1Mn0.2O2 cell assembled with the composite cathode employing NBR25 exhibited an initial discharge capacity of 149.0 mAh g−1 with good capacity retention at 0.2 C and 25 °C.
Files in This Item
Go to Link
Appears in
Collections
서울 공과대학 > 서울 화학공학과 > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Kim, Dong Won photo

Kim, Dong Won
COLLEGE OF ENGINEERING (DEPARTMENT OF CHEMICAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE