Quantitative analysis of polystyrene microplastic and styrene monomer released from plastic food containersopen access

Authors
Wang, JiaeLee, JieunKwon, Eilhann E.Jeong, Sanghyun
Issue Date
May-2023
Publisher
Elsevier Ltd
Keywords
Fourier-transformed infrared spectroscopy; Microplastics; Plastic container; Polystyrene; Simultaneously exposed pollutant; Styrene
Citation
Heliyon, v.9, no.5, pp.1 - 13
Indexed
SCIE
SCOPUS
Journal Title
Heliyon
Volume
9
Number
5
Start Page
1
End Page
13
URI
https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/192484
DOI
10.1016/j.heliyon.2023.e15787
Abstract
Since the COVID-19 outbreak, the use of disposable plastics has rapidly increased along with the amount of plastic waste. During fragmentation, microplastics and other chemical substances contained in plastics are released. These then enter humans through food which could be problematic considering their hazardous potential. Polystyrene (PS), which is widely used in disposable containers, releases large amounts of microplastics (MPs), but no studies have investigated the release mechanisms of PS-MPs and simultaneously exposed contaminants. Therefore, in this study, the effects of pH (3, 5, 7, and 9), temperature (20, 50, 80, and 100 °C), and exposure time (2, 4, 6, and 8 h) on MPs release were systematically examined. A quantitative/qualitative study of MPs and styrene monomers was performed using microscopy-equipped Fourier-transformed infrared spectroscopy and gas chromatography-mass spectrometry. The release of PS-MPs (36 items/container) and simultaneously exposed pollutants (SEP), such as ethylene glycol monooleate (EGM), was highest at pH 9, 100 °C, and 6 h, which was proportional to the test temperature and time. Under the same conditions, 2.58 μg/L of styrene monomer migrated to the liquid food simulants. The fragmentation was proceeded by oxidation/hydrolysis and accelerated by increased temperature and exposure time. The strong positive correlation between PS-MPs and SEPs releases at pH and temperature indicates that PS-MPs and SEPs follow the same release process. However, a strongly negative correlation between PS-MPs and styrene monomers at the exposed time shows that styrene migration does not follow the same release process, but does its partition coefficient.
Files in This Item
Appears in
Collections
서울 공과대학 > 서울 자원환경공학과 > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Kwon, Eilhann E. photo

Kwon, Eilhann E.
COLLEGE OF ENGINEERING (DEPARTMENT OF EARTH RESOURCES AND ENVIRONMENTAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE