Detailed Information

Cited 1 time in webofscience Cited 2 time in scopus
Metadata Downloads

Dehydrogenation of 2-[(n-Methylcyclohexyl)Methyl]Piperidine over Mesoporous Pd-Al₂O₃ Catalysts Prepared by Solvent Deficient Precipitation: Influence of Calcination Conditionsopen access

Authors
Bathula, Hari BabuOh, JinhoJo, YeonginSuh, Young-Woong
Issue Date
Sep-2019
Publisher
MDPI
Keywords
dehydrogenation; liquid organic hydrogen carrier; solvent deficient precipitation; mesoporous Pd-Al2O3; calcination condition
Citation
CATALYSTS, v.9, no.9, pp.1 - 19
Indexed
SCIE
SCOPUS
Journal Title
CATALYSTS
Volume
9
Number
9
Start Page
1
End Page
19
URI
https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/32827
DOI
10.3390/catal9090719
ISSN
2073-4344
Abstract
A pair of 2-[(n-methylcyclohexyl)methyl]piperidine (H-12-MBP) and its full dehydrogenation product (H-0-MBP) has recently been considered as a potential liquid organic hydrogen carrier with 6.15 wt% H-2 storage capacity. In the discovery of an active and stable catalyst for H-2 discharge from H-12-MBP at lower temperatures, a mesoporous Pd-Al2O3 catalyst (MPdA) was synthesized by a one-pot solvent deficient precipitation (SDP). In the present work, the sensitivity and effectiveness of the SDP method are examined by varying the calcination temperature and time in the preparation of the MPdA catalyst. The characterization revealed that the final properties of the MPdA catalyst greatly rely on both the calcination temperature and time. The MPdA catalyst showed better dehydrogenation activity for calcination at 600 degrees C than at other temperatures, because of Pd particles of smaller size with higher dispersion. Although the MPdA catalysts calcined at 600 degrees C for different periods of time have similar size and dispersion of Pd particles, the dehydrogenation efficiency was superior as the calcination time became shorter (e.g., 1 h), which originated from the better arrangement of Pd particles over a higher surface area. These MPdA catalysts, irrespective of the calcination time, displayed a remarkable stability in the dehydrogenation of H-12-MBP owing to the protection of Pd particles by the Al2O3 layer.
Files in This Item
Appears in
Collections
서울 공과대학 > 서울 화학공학과 > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Suh, Young Woong photo

Suh, Young Woong
COLLEGE OF ENGINEERING (DEPARTMENT OF CHEMICAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE