하이드로 피어싱 시험을 통한 구멍 주위의 꺼짐 현상 분석Study of Deflection around Hydropierced Hole with Experiment

Other Titles
Study of Deflection around Hydropierced Hole with Experiment
Authors
한수식강연식김근환
Issue Date
2007
Publisher
한국소성가공학회
Keywords
Sheared Ege; Internal Pessure; Hydroforming; Rollover; Tapered Pnch; Sheared Ege; Internal Pessure; Hydroforming; Rollover; Tapered Pnch
Citation
소성가공, v.16, no.3, pp 157 - 162
Pages
6
Journal Title
소성가공
Volume
16
Number
3
Start Page
157
End Page
162
URI
https://scholarworks.bwise.kr/kumoh/handle/2020.sw.kumoh/22865
ISSN
1225-696X
2287-6359
Abstract
The hydropiercing process gives a lot of advantages to the tube hydroforming such as cost reduction and high productivity. However it has a drawback, the amount of deflection around the hole is bigger than that of conventional die piercing process. The deflection can cause the problem at the assembly process of stamped parts and hydroformed part. Therefore the reduction of deflection is one of the most important issues for hydropiercing process. In this study, the deflection around hydropierced hole was investigated by experiment. As a result of investigation, the amount of deflection is influenced by the internal pressure, the material thickness and the size of hole. Especially the hole size is most influencing factor on the deflection around the hydropierced hole.
Files in This Item
There are no files associated with this item.
Appears in
Collections
Department of Mechanical Engineering > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Altmetrics

Total Views & Downloads

BROWSE