Detailed Information

Cited 0 time in webofscience Cited 0 time in scopus
Metadata Downloads

Reliability evaluation of QFP solder joint using Sn-8Zn-3Bi solder paste during the thermal shock test

Authors
Han, S. W.Chang, K. H.Han, J. G.Cho, I. J.Kim, J. M.Choi, M. G.Kim, Y. T.Shin, Y. E.
Issue Date
Jun-2008
Publisher
TRANS TECH PUBLICATIONS LTD
Keywords
Sn-Zn-Bi solder; Quad flat package (QFP); intermetallics; pull strength; thermal shock; fracture mode
Citation
ADVANCED WELDING AND MICRO JOINING / PACKAGING FOR THE 21ST CENTURY, v.580-582, pp 247 - +
Journal Title
ADVANCED WELDING AND MICRO JOINING / PACKAGING FOR THE 21ST CENTURY
Volume
580-582
Start Page
247
End Page
+
URI
https://scholarworks.bwise.kr/cau/handle/2019.sw.cau/54430
DOI
10.4028/www.scientific.net/MSF.580-582.247
ISSN
0255-5476
Abstract
The reliability of QFP Quad flat package) solder joint using Sn-8Zn-3Bi solder paste under the thermal shock test was investigated. Considering the environmental restriction such as ROHS, the QFP Cu LF (Lead-frame) was coated with lead-free materials (Sri, Sn-3Bi). To analyze the reliability under thermal shock treatment, the samples were placed in the thermal shock chamber (248K/423K, Dwell time: 30min). During the thermal shock test, the solder Joint cross-sections were observed every 500 cycles. No crack initiation and propagation was observed through all type of plated Cu LF. The measured pull strength slightly decreased, as the number of cycles increased. After 1000 cycles, the pull strength of Sri and SnBi plated Cu LF reduced by 30% and 20%, respectively, compared with that of initial condition. Observing the fracture surface morphology by FE-SEM, the fracture mode changed and the IMC fractured area on the both fracture Surface was increased. The IMC was identified as gamma-Cu5Zn8 by chemical composition analysis using EDS. The reduced pull strength was affected by IMC fracture and fracture mode change. However, the pull strength does not decrease steeply but gradually. Consequently, the Sn-8Zn-3Bi solder Joint shows the reliable solder joint strength, fracture mechanism, and compatibility with lead-free plated Cu LF during the thermal shock temperature of 248K to 423K.
Files in This Item
There are no files associated with this item.
Appears in
Collections
College of Engineering > School of Mechanical Engineering > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Han, Jung Geun photo

Han, Jung Geun
공과대학 (건설환경플랜트공학)
Read more

Altmetrics

Total Views & Downloads

BROWSE