Optimization of crack-free polytypoidally joined Si3N 4-Al2O3 functionally graded materials (FGM) using 3-dimensional modeling

Authors
Ryu, Sae-HeePark, Jong-HaLee, Caroline SunyongLee, Jae-ChulAhn, Sung-HoonChae, Jae-HongRiu, Doh-Hyung
Issue Date
Dec-2007
Publisher
Trans Tech Publications
Keywords
FEM (finite element method); FGM (functionally graded materials); Hot press; Oriented Vickers indentation test; Polytypoid; Si3N4-Al2O3 joining
Citation
Advanced Materials Research, v.47-50 PART 1, pp 494 - 498
Pages
5
Indexed
SCIE
SCOPUS
Journal Title
Advanced Materials Research
Volume
47-50 PART 1
Start Page
494
End Page
498
URI
https://scholarworks.bwise.kr/erica/handle/2021.sw.erica/43066
DOI
10.4028/www.scientific.net/AMR.47-50.494
ISSN
1022-6680
1662-8985
Abstract
Joining Si3N4 and Al2O3 using 15 layers has been achieved by a unique approach that introduces SiAlON polytypoids as a functionally graded material (FGM) bonding layer. Previously, the hot press sintering of multilayered FGM with 20 layers, each 500 μ thick, has been achieved successfully. In the present study, the number of layers for FGM was reduced from 20 to 15 to increase optimization. Samples were fabricated by hot pressing at 48 MPa during the temperature ramp to 1650°C and cooling at 2°C/min to minimize residual stresses from sintering. Moreover, a finite element method (FEM) program based on the maximum principal stress theory and the maximum tensile stress theory was applied to design optimized and reduced FGM layers that produced a crack-free joint. The sample had a 3-dimensional cylindrical shape that was transformed to a 2-dimensional axisymmetric mode. By determining the expected thermal stress from the calculated elastic modulus and coefficient of thermal expansion, we were able to predict and prevent damage due to thermal stresses. These analyses are especially useful for FGM samples where it is very difficult to measure the residual stresses experimentally. Finally, oriented Vickers indentation testing was used to qualitatively characterize the strengths of the joint and the various interfaces. The indentation cracks were deflected at the SiAlON layers, implying weak interfaces. In other areas, cracks were not deflected, implying strong interfaces. © 2008 Trans Tech Publications.
Files in This Item
Go to Link
Appears in
Collections
COLLEGE OF ENGINEERING SCIENCES > DEPARTMENT OF MATERIALS SCIENCE AND CHEMICAL ENGINEERING > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Lee, Sunyong Caroline photo

Lee, Sunyong Caroline
ERICA 공학대학 (DEPARTMENT OF MATERIALS SCIENCE AND CHEMICAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE