Improvement of imaging properties by optimizing the capping structure in extreme ultraviolet lithography

Authors
Jeong, Chang YoungLee, SangsulShin, Hyun-DuckKim, Tae GeunAhn, Jinho
Issue Date
Nov-2009
Publisher
A V S AMER INST PHYSICS
Keywords
image processing; molybdenum; molybdenum alloys; phase shifting masks; ruthenium; silicon; silicon alloys; tantalum compounds; ultraviolet lithography
Citation
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B, v.27, no.6, pp.2922 - 2926
Indexed
SCIE
SCOPUS
Journal Title
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY B
Volume
27
Number
6
Start Page
2922
End Page
2926
URI
https://scholarworks.bwise.kr/hanyang/handle/2021.sw.hanyang/175924
DOI
10.1116/1.3246358
ISSN
1071-1023
Abstract
The optimization of capping structure for extreme ultraviolet lithography was conducted to minimize the mask shadowing effect. The capping structure used in this study consisted of a phase shift layer and a capping layer on the 40 pairs of Mo-Si multilayer. A phase shift layer was added below tantalum nitride (TaN) absorber pattern. The authors analyzed the effect of the following capping materials such as ruthenium (Ru), silicon (Si), and molybdenum (Mo) with thickness variation. TaN absorber thickness for out-of phase condition shifted with the capping layer thickness change. The variation in capping materials showed less of an effect compared to thickness change. The addition of phase shift layer below absorber pattern showed a significant effect on the phase difference. Ru phase shift layer with a higher delta value than TaN absorber, shifted phase difference to the positive direction, whereas Si phase shift layer with a lower delta value than TaN absorber, shifted phase difference to the negative direction. However, phase difference was not shifted by the addition of Mo phase shift layer which has a similar delta value with TaN absorber. We also calculated the horizontal-vertical overlapping process window according to Mo phase shift layer thickness using 22 nm 1:1 line and space pattern. As Mo phase shift layer thickness increased, the overlapping zone in the exposure latitude of the focus-exposure plots between the horizontal and vertical features increased.
Files in This Item
Go to Link
Appears in
Collections
서울 공과대학 > 서울 신소재공학부 > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Ahn, Jinho photo

Ahn, Jinho
COLLEGE OF ENGINEERING (SCHOOL OF MATERIALS SCIENCE AND ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE