Influence of a wrinkle in terms of critical dimension variation caused by transmission nonuniformity and a particle defect on extreme ultraviolet pellicle

Authors
Kim, Guk-JinKim, In-SeonLee, Sung-GyuYeung, MichaelKim, Min-SuPark, Jin-GooOh, Hye-Keun
Issue Date
Oct-2017
Publisher
SPIE - International Society for Optical Engineering
Keywords
extreme ultraviolet pellicle; pellicle deformation; wrinkle and particle defect on extreme ultraviolet pellicle
Citation
Journal of Micro/ Nanolithography, MEMS, and MOEMS, v.16, no.4
Indexed
SCIE
SCOPUS
Journal Title
Journal of Micro/ Nanolithography, MEMS, and MOEMS
Volume
16
Number
4
URI
https://scholarworks.bwise.kr/erica/handle/2021.sw.erica/8954
DOI
10.1117/1.JMM.16.4.041008
ISSN
1932-5150
Abstract
An extreme ultraviolet (EUV) pellicle is needed for the protection of EUV masks from defects, contaminants, and particles during the exposure process. However, the EUV pellicle can be easily deformed during the exposure process because it has an extremely thin thickness for high transmission of EUV lights. Due to the very thin thickness and the weak structure of the pellicle, a pellicle is easily deformed; a wrinkled pellicle causes an image distortion, which leads to critical dimension (CD) variation. In addition, a particle defect on an EUV pellicle can result from scanner building materials. Added materials of the particle defect on an EUV pellicle can also cause image distortion and CD variation. We investigated the impact of wrinkles and particle defects on the transmission and CD variation for the 5- and 3-nm nodes of isomorphic and anamorphic numerical aperture (NA) systems. The variation in transmission and the critical size of the particle defect with a wrinkled EUV pellicle were calculated to obtain the requirement of a CD variation of 0.2 nm for a EUV pellicle. As a result, a change in transmission of 1.9% (after two pass) resulted in a 0.2-nm variation in the CD for the anamorphic NA system (3-nm node), whereas a transmission variation of 1.3% (after two pass) caused a 0.2-nm CD variation in the isomorphic NA system (5-nm node). From these results, an allowable local tilt angle can be calculated; the allowable local tilt angle of an isomorphic NA system is 0.31 rad and that of an anamorphic NA system is 0.41 rad. When the particle defect is added on a wrinkled EUV pellicle, the critical size of the particle defect is 1.2 mu m for the 5-nm node and 2.2 mu m for the 3-nm node. (c) 2017 Society of Photo-Optical Instrumentation Engineers (SPIE)
Files in This Item
Go to Link
Appears in
Collections
COLLEGE OF SCIENCE AND CONVERGENCE TECHNOLOGY > DEPARTMENT OF APPLIED PHYSICS > 1. Journal Articles
COLLEGE OF ENGINEERING SCIENCES > DEPARTMENT OF MATERIALS SCIENCE AND CHEMICAL ENGINEERING > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Park, Jin Goo photo

Park, Jin Goo
ERICA 공학대학 (DEPARTMENT OF MATERIALS SCIENCE AND CHEMICAL ENGINEERING)
Read more

Altmetrics

Total Views & Downloads

BROWSE